1. PP油墨適用范圍:適用于PP、PET、PE、BOPP等制品。2. 油墨特性:固化后對極性底材具有優(yōu)異的附著力,防汽油、白電油及正己烷效果特別好(用汽油擦30次或汽油浸泡15秒不脫落,同時可耐酒精和手汗);墨層均勻,顏料分散性好,不干網(wǎng),過網(wǎng)性、流平性良好,涂膜具有較高的硬度、光澤及良好的耐水性、耐候性、耐化學(xué)藥品性;印刷方便,可以絲印和移??!3. 油墨技術(shù)參考粘度:5000-15000CPS(因溫度、顏色而異)細度:5um↓附著力:5B優(yōu)自干:25℃時,24小時固化;烘干:60℃時,30分鐘固化過網(wǎng)性能:200目-400目網(wǎng)紗(用金、銀、珠光粉調(diào)配之油墨除外)稀釋劑:L-007中干水涂覆面積:30-35㎡/㎏(測試以300目聚脂單絲感光膠、網(wǎng)版為標準)4. 油墨使用方法根據(jù)需要,部分材料可添加WG-005固化劑5-10%,以便增強附著性。印刷前需要用WJ-003處理劑擦拭,以加強耐汽油效果和附著力。受到污染的素材應(yīng)在表面用去漬油清洗或擦拭,以利于印刷效果優(yōu)異。印刷錯誤時,應(yīng)待其未完全干燥前用抹字水去除,重新再印。印刷過程中遇到網(wǎng)版堵塞之狀況,應(yīng)先用洗版水清洗之后再印刷。需要套色時,應(yīng)在前顏色表干或硬干后再進行套色工作。附著力、硬度、耐酸性、耐油性、耐去漬油性、抗劃傷性、耐磨性等性能的檢測,需要墨層完全固化后方可檢測。未經(jīng)允許,不得將PCA系列油墨與其它類型油墨混用及配色。1. PP-ink application: suitable for PP, PET, PE, BOPP and other products. 2. ink characteristics: curing Hou on polar late material has excellent of adhesion, anti-gasoline, and white electric oil and the are himself n-effect special good (with gasoline wipe 30 times or gasoline soaking 15 seconds not shedding, while can resistance alcohol and hand Khan); ink layer uniform, pigment dispersion good, not dry network, had network sex, and flow flat sex good, coated film has high of hardness, and gloss and the good of resistance waterborne, and resistance waiting sex, and resistance chemical drug sex; printing convenient, can silk printed and moved printed! 3. ink technology reference stick degrees: 5000-15000CPS (due to temperature, and color and ISO) fine degrees: 5um ↓ adhesion: 5B excellent since dry: 25 ℃ Shi, 24 hours curing; drying: 60 ℃ Shi, 30 minutes curing had network performance: 200 accounts-400 accounts network yarn (with gold, and silver, and Pearlescent powder deployment of ink except) diluted agent: L-007 in the dry water coated reply area: 30-35 square meters/kg (test to 300 accounts poly fat single silk photographic glue, and network version for standard) 4. Ink usage based on need, some materials can add curing agent 5–10% WG-005, in order to enhance adhesiveness. Wipe with a WJ-003 treatment agent required prior to printing to enhance gasoline resistance and adhesion effect. Contaminated materials should be cleaned with oil stains on the surface or wipe in order to facilitate the printing effect is excellent. When an error is printed, which are not fully dry before using the word water removal, start printing. Encountered in the print screen blocking should be printed after the first wash with washing water. When a registration is required, you should color table before doing color work or hard dried. Adhesion, hardness, resistance to acid oil, oil resistance, stain resistance, scratch resistance, abrasion resistance and other properties of the test, need to be fully cured ink layer before the test. Without permission, PCA series ink may not be mixed with other types of ink and color matching.